募捐 9月15日2024 – 10月1日2024 关于筹款

Creep Properties of Heat Resistant Steels and Superalloys

Creep Properties of Heat Resistant Steels and Superalloys

T.-U. Kern, G. Merckling, K. Yagi (auth.), K. Yagi, G. Merckling, T.-U. Kern, H. Irie, H. Warlimont (eds.)
你有多喜欢这本书?
下载文件的质量如何?
下载该书,以评价其质量
下载文件的质量如何?

For environmental reasons it is necessary to increase the process temperature in power plants and in industry, e.g. in chemical plants. This implies the development of steels and alloys that can be used at high temperatures and severe conditions. These materials need to be capable of enduring long-term use. On the other hand, equipment and plants built in the 1970s have become aged and their control requires a high degree of accuracy to ensure their safe operation. In this case, the most important property of the materials is creep, especially long-term creep, and thus it is necessary to evaluate and estimate long-term creep strength more accurately. It is therefore a top priority to accumulate data and knowledge about creep and to share the information.

This volume contains a compilation of long-term creep and rupture data and knowledge based on these data on heat resistant steels and superalloys, collected by three leading creep research organizations and agencies, namely: ECCC (European Creep Collaborative Committee), GCC (German Creep Committee) and NIMS (National Institute for Materials Science) of Japan.

种类:
年:
2004
出版:
1
出版社:
Springer-Verlag Berlin Heidelberg
语言:
english
页:
365
ISBN 10:
354045599X
ISBN 13:
9783540455998
系列:
Landolt-Börnstein - Group VIII Advanced Materials and Technologies 2B : Advanced Materials and Technologies
文件:
PDF, 21.11 MB
IPFS:
CID , CID Blake2b
english, 2004
线上阅读
正在转换
转换为 失败

关键词